Cracks in Render
Low risk · Fixed by a plasterer
What's happening?
Render is bonded to the wall, so it cannot be treated as flexible: any movement in the wall behind shows up in it. Sika's technical sheet says hairline cracks under 0.2mm may appear as the render cures, are classed as fissure cracks and are acceptable under BS EN 13914. Wider cracks are also not detrimental to the system but should be inspected, because they are typically caused by movement in the wall behind, such as settlement in a new structure. Once that has settled, they can be repaired and should not return. If they do not settle, the movement is more serious. The most common causes Sika finds on site are a lack of bed joint reinforcement and no movement joints. On old solid walls, SPAB warns that strong cement renders form hair cracks as they set and let moisture in by capillary action.
What usually causes it?
- Surface shrinkage as the render cures, which gives hairline fissure cracks under 0.2mm
- A lack of bed joint reinforcement in the block or brick behind, which cracks render diagonally from window and door corners
- A lack of movement joints, which causes vertical cracks in the render
- Movement in the structure behind, such as settlement of a new building or ground movement and frost heave
- An excessively wet background or render applied to a wet wall
- Strong cement render on an old solid wall, which SPAB says forms hair cracks as it sets and then lets moisture in
Is it dangerous?
Render cracks are not a safety risk in themselves, but a wide or growing crack means the wall behind is moving and Sika says that is more serious. Check whether a crack follows the line of the blocks or runs from a window corner before you fill it, because the pattern points at the cause.
Can I fix it myself?
1. Measure the crack. Under 0.2mm is a hairline from curing. 2. Note whether it is vertical, diagonal from a window or door corner, or follows the block courses, because the pattern points at the cause. 3. Check the gutters and downpipes above for leaks that keep the wall wet, and fix them first. 4. Leave a crack that is still opening, because filling it only moves the problem. 5. Once a crack is stable, repair it with a product made for masonry coatings, as Sika advises.
When should you call a plasterer?
Call a plasterer or renderer if cracks are wider than hairline, form a pattern, let in water, or the render sounds hollow. Call a surveyor if the cracks keep growing after being repaired. On an old solid wall, a plasterer who works in lime should say whether the render should be replaced with a breathable one.
What will the plasterer actually do?
- Map the cracks and tap the render to find hollow or detached areas
- Fix the water source, such as a leaking gutter or pipe, before repairing the render
- Repair stable cracks using a crack repair method suited to the coating and render type
- Cut out and re-render failed areas, with reinforcing mesh where it was missing
- Recommend or form movement joints where the wall design calls for them
Who fixes this
- External rendering repair
- External wall rendering
Questions people ask
Are hairline cracks in render normal?
What causes wider cracks in render?
Why does cement render crack on an old house?
Can I just fill a crack in render?
Sources & References
Before you book, read how to check a tradesman is legit.