Skip to main content
Crack Between the Ceiling and the Wall

Crack Between the Ceiling and the Wall

A thin, even crack along the top of a wall is usually shrinkage or thermal movement, and a crack over 5mm, wedge-shaped, or growing needs someone to look at it.

Low risk · Fixed by a plasterer

Updated

What's happening?

Walls and ceilings are built from different materials that respond to heat and moisture differently, so the joint between them is a natural place for a crack. NHBC says shrinkage cracks often run along the wall near the ceiling or near the floor at a constant width, normally under 2mm, and thermal movement cracks are common where an external wall joins an internal plasterboard wall or where boards join on a plasterboard ceiling. Hairline cracks may also show on ceilings under the joists. A crack of 2mm or less is considered cosmetic and can be repaired with a suitable filler, grout or sealant. If it reappears after a year or so, that is likely to be thermal movement, unless it keeps getting wider. The width and the pattern tell you which case you have.

What usually causes it?

  • Shrinkage as plaster, mortar and other wet-built materials dry out, which usually leaves a crack of constant width under 2mm
  • Thermal movement, as different materials expand and contract at different rates through the seasons
  • Plasterboard joints on a ceiling, where boards meet and move slightly
  • Moisture movement, as materials absorb and release moisture through the year
  • Settlement of a newer home on its foundations, which usually settles quickly
  • Ground movement, which NHBC says tends to give cracks that are wide at one end and narrow at the other

Is it dangerous?

Most such cracks are cosmetic and unlikely to affect stability. NHBC advises contacting them or getting an assessment if a crack is wider than 5mm at any point, is wide at one end and narrow at the other, is diagonal or stepped, is visible inside and outside, has got wider or longer since you noticed it, or comes with doors and windows that start to stick.

Can I fix it myself?

1. Measure the crack at its widest. NHBC suggests the edge of a one pound coin, about 3mm, if you have no ruler. 2. Note the date, take a photo with the ruler or coin beside it, and check it again in a few weeks. 3. If it is 2mm or less and not changing, clean out the dust and fill it with a suitable flexible filler or sealant, then repaint. 4. Look for matching cracks outside, in the same position on the other side of the wall. 5. If it is wider than 5mm, wedge-shaped or growing, stop filling and get it assessed.

When should you call a plasterer?

Call a plasterer to repair a stable crack, to re-run a cracked joint or to fit coving or cornice over a joint that keeps opening. Get a surveyor or structural engineer first if it is wider than 5mm, wide at one end, diagonal, visible outside as well, or still growing.

What will the plasterer actually do?

  • Check the crack's width and pattern and whether the plaster nearby is hollow or loose
  • Rake out the crack and re-fill or re-tape the joint with a material that tolerates movement
  • Cut out and re-plaster loose areas where the plaster has lost adhesion
  • Fit coving or cornice over a joint that keeps opening, where that suits the room
  • Prepare the surface for decorating, and advise on a structural check if the crack suggests movement

Who fixes this

  • Wall and ceiling repairs
  • Coving and cornice

Questions people ask

Why is there a crack where my ceiling meets the wall?

NHBC says shrinkage and thermal movement are the usual causes, particularly where an external wall meets an internal plasterboard wall and where plasterboard boards join on a ceiling.

How wide is too wide?

NHBC says a crack of 2mm or less is cosmetic, and says to contact them if it is wider than 5mm at any point, is wedge-shaped, is diagonal or stepped, or keeps getting wider.

Why does the crack keep coming back after filling?

NHBC says a crack that reappears after a year or so is likely to be thermal movement, and is nothing to worry about unless it keeps getting wider.

Does paint crack along the joint too?

Dulux says excessive movement of the surface under paint, such as at joints, stresses the paint film and can crack it, which then lets moisture in and can lead to flaking.

Sources & References

  1. NHBC: cracking in your home
  2. Dulux: 15 paint problems and how to fix them

Need a plasterer?

Describe the job and get a fixed price from a local plasterer.